NASA Licenses 3D-Printable High-Temperature Superalloy That Can Last 2,500x Longer


NASA's superalloy GRX-810, designed for extreme air and spaceflight conditions, is now being licensed to four American companies, enhancing the U.S. economy through improved aerospace components. This 3D-printable material increases the durability of parts, withstands severe temperatures, and promot